Wrought alloy (bar, rod, sheet, forging) · Germany · DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672
2.0742 CuNi18Zn27
2.0742 (CuNi18Zn27) is a wrought cu-ni-zn alloy to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN, in the nickel silver group. Nominal composition: Cu 53.5-56.5, Ni 16.5-19.5, Zn rem. Typical uses: springs, contacts, musical instruments. Equivalents: C77000 (USA), CW410J CuNi18Zn27 (Europe), NS107 (UK), C7701 (Japan).
Conex Casting Foundry — Alloy datasheet
sales@casting-foundry.in · +91-22-43449300 · casting-foundry.in/alloys/din-2-0742
2.0742 CuNi18Zn27
DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN
Chemical composition
2.0742 — nominal composition
Weight %, to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN. Single values are maximums unless marked. The full limits (impurities) are in the standard.
| Element | Weight % |
|---|---|
| Cu | 53.5-56.5 |
| Ni | 16.5-19.5 |
| Zn | rem |
Mechanical & physical properties
2.0742 — properties
Values shown are for C77000, the same alloy in another standard. Limits for 2.0742 may differ slightly — the standard on your drawing governs.
| Tensile strength, typical | 420 MPa |
| Yield / 0.2 % proof stress, typical | 185 MPa |
| Elongation, typical | 40 % |
| Brinell hardness, typical | 85 HB |
| Density at 20 °C | 8.7 g/cm³ |
| Melting range (solidus–liquidus) | 1020–1055 °C |
| Electrical conductivity at 20 °C | 5.5 % IACS |
| Thermal conductivity at 20 °C | 29 W/m·K |
Source: annealed, CDA / ASM handbook (typical values).
International equivalents
2.0742 cross-reference
| System | Designation |
|---|---|
| Germany (this grade) | 2.0742 · CuNi18Zn27 |
| USA · UNS / ASTM | C77000 |
| Europe · EN | CW410J CuNi18Zn27 |
| UK · BS | NS107 |
| Japan · JIS | C7701 |
| China · GB | — |
⚠️ Relationship: Direct. Equivalents are the closest published matches — composition and property limits can differ slightly between standards, and cast and wrought grades are never interchangeable. The standard on your drawing governs.
Typical applications
- ▸ Springs
- ▸ Contacts
- ▸ Musical instruments
Product forms: Rod, bar, wire, sheet, strip, tube
2.0742 parts
2.0742 is a wrought grade (bar, rod, forging): we supply parts CNC machined from bar or forged — it is not used for castings. For a cast part, choose a cast grade.
Same alloy in other standards
Grades from the same cross-reference group.
Specification
How to specify 2.0742 on a drawing or order
- ▸ Grade and standard: DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 – 2.0742 / CuNi18Zn27.
- ▸ Temper and size: state the temper (for example R360 / H080) when strength or hardness matters.
- ▸ Certificates: EN 10204 3.1 material test certificate per lot; dimensional report on request.
- ▸ Files: a PDF drawing plus a STEP model gives the fastest quotation.
Buyer guides: EN 10204
2.0742 — questions buyers ask
What is 2.0742?+
2.0742 (CuNi18Zn27) is a wrought cu-ni-zn alloy to DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN, in the nickel silver group. Nominal composition: Cu 53.5-56.5, Ni 16.5-19.5, Zn rem. Typical uses: springs, contacts, musical instruments. Equivalents: C77000 (USA), CW410J CuNi18Zn27 (Europe), NS107 (UK), C7701 (Japan).
What are the equivalents of 2.0742?+
USA: C77000; Europe: CW410J CuNi18Zn27; UK: NS107; Japan: C7701. Relationship: Direct. Equivalents are close matches — composition and property limits can differ between standards, so always confirm against the standard on your drawing.
What is the tensile strength of 2.0742?+
Tensile strength, typical: 420 MPa; Yield / 0.2 % proof stress, typical: 185 MPa; Elongation, typical: 40 %; Brinell hardness, typical: 85 HB. Source: annealed, CDA / ASM handbook (typical values).
Does Conex supply parts in 2.0742?+
2.0742 is a wrought grade (bar, rod, sheet or forging stock). We machine and supply finished parts in it to your drawing, and can recommend the matching cast grade if you need a casting instead.
How do I specify 2.0742 on a drawing?+
Write the standard and the grade together, for example "DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 – 2.0742 (CuNi18Zn27)", and the temper. Ask for an EN 10204 3.1 material test certificate if you need lot traceability.
Sources & references
- ▸ Grade, composition and cross-reference: Conex international alloy master (USA UNS/ASTM, EN, DIN, BS, JIS, GB), reviewed October 2026.
- ▸ Controlling standard: DIN 17660 / 17662 / 17663 / 17664 / 17666 / 17672 (legacy) - now DIN EN — Legacy DIN designation (W.Nr still widely quoted).
- ▸ Properties: annealed, CDA / ASM handbook (typical values).
- ▸ Always verify against the current edition of the standard for contract or safety-critical parts.
Order 2.0742
Indicative $16/kg · from 100 kg, any quantity · Any variation, we will confirm final price on quotation
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.