36 grades · 36 wrought
Free-Cutting & Forging Brass
Leaded brasses for CNC turning, hot stamping and forging (CZ121, CW614N, CW617N, C36000). 36 grades across USA, European, German, British, Japanese and Chinese standards — each with its own datasheet and cross-reference.
36 of 36 grades
| Grade | Name | System | Form | Composition |
|---|---|---|---|---|
| C34000● data | Low-leaded brass 1Pb | USA · UNS / ASTM B121, B453 | Wrought | Cu 62-65, Pb 0.8-1.5, Zn rem |
| CW600N● data | CuZn35Pb1 | Europe · EN 1412 numbering | Wrought | Cu 62-64, Pb 0.8-1.6, Zn rem |
| CZ118● data | Low-leaded brass 1Pb | UK · BS 2870-2875 | Wrought | Cu 62-64, Pb 0.8-1.6, Zn rem |
| C3501● data | Low-leaded brass 1Pb | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu 62-64, Pb 0.8-1.6, Zn rem |
| 2.0331● data | CuZn36Pb1.5 | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu 62-64, Pb 0.8-1.6, Zn rem |
| C34200● data | Medium-leaded brass 2Pb | USA · UNS / ASTM B121, B453 | Wrought | Cu 62-65, Pb 1.5-2.5, Zn rem |
| C35300● data | Medium-leaded brass 2Pb | USA · UNS / ASTM B121, B453 | Wrought | Cu 60-63, Pb 1.5-2.5, Zn rem |
| CW601N● data | CuZn35Pb2 | Europe · EN 1412 numbering | Wrought | Cu 62-64, Pb 1.6-2.5, Zn rem |
| CZ119● data | Medium-leaded brass 2Pb | UK · BS 2870-2875 | Wrought | Cu 62-64, Pb 1.6-2.5, Zn rem |
| C36000● data | Free-cutting brass 60/3 (alloy 360) | USA · UNS / ASTM B16, B124 | Wrought | Cu 60-63, Pb 2.5-3.7, Fe <= 0.35, Zn rem |
| CW603N● data | CuZn36Pb3 | Europe · EN 1412 numbering | Wrought | Cu 60-63, Pb 2.5-3.7, Fe <= 0.35, Zn rem |
| 2.0375● data | CuZn36Pb3 | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu 60-63, Pb 2.5-3.7, Fe <= 0.35, Zn rem |
| CZ124● data | Free-cutting brass 60/3 (alloy 360) | UK · BS 2870-2875 | Wrought | Cu 60-63, Pb 2.5-3.7, Fe <= 0.35, Zn rem |
| C3601● data | Free-cutting brass 60/3 (alloy 360) | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu 60-63, Pb 2.5-3.7, Fe <= 0.35, Zn rem |
| C3602● data | Free-cutting brass 60/3 (alloy 360) | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu 60-63, Pb 2.5-3.7, Fe <= 0.35, Zn rem |
| C35000● data | Riveting / cold-heading leaded brass | USA · UNS / ASTM B121, B453 | Wrought | Cu 60-63, Pb 0.8-2.0, Zn rem |
| CW606N● data | CuZn37Pb2 | Europe · EN 1412 numbering | Wrought | Cu 61-64, Pb 1.6-2.5, Zn rem |
| CZ131● data | Riveting / cold-heading leaded brass | UK · BS 2870-2875 | Wrought | Cu 61-64, Pb 1.6-2.5, Zn rem |
| C3713● data | Riveting / cold-heading leaded brass | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu 61-64, Pb 1.6-2.5, Zn rem |
| CW608N● data | CuZn38Pb2 | Europe · EN 1412 numbering | Wrought | Cu 60-61, Pb 1.6-2.5, Zn rem |
| 2.0371● data | CuZn38Pb1.5 | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu 60-61, Pb 1.6-2.5, Zn rem |
| CZ128● data | Leaded brass 38/2 | UK · BS 2870-2875 | Wrought | Cu 60-61, Pb 1.6-2.5, Zn rem |
| C37700● data | Leaded brass 38/2 | USA · UNS / ASTM B124 | Wrought | Cu 58-61, Pb 1.5-2.5, Fe <= 0.3, Zn rem |
| CW612N● data | CuZn39Pb2 | Europe · EN 1412 numbering | Wrought | Cu 59-60, Pb 1.6-2.5, Zn rem |
| 2.0380● data | CuZn39Pb2 | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu 59-60, Pb 1.6-2.5, Zn rem |
| C3771● data | Forging brass 39/2 | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu 59-60, Pb 1.6-2.5, Zn rem |
| C38500● data | Free-machining brass 58/3 (CZ121) | USA · UNS / ASTM B455, B124 | Wrought | Cu 55-59, Pb 2.5-3.5, Fe <= 0.35, Zn rem |
| CW614N● data | CuZn39Pb3 | Europe · EN 1412 numbering | Wrought | Cu 57-59, Pb 2.5-3.5, Fe <= 0.3, Zn rem |
| 2.0401● data | CuZn39Pb3 | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu 57-59, Pb 2.5-3.5, Fe <= 0.3, Zn rem |
| CZ121● data | Free-machining brass 58/3 (CZ121) | UK · BS 2870-2875 | Wrought | Cu 57-59, Pb 2.5-3.5, Fe <= 0.3, Zn rem |
| C3603● data | Free-machining brass 58/3 (CZ121) | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu 57-59, Pb 2.5-3.5, Fe <= 0.3, Zn rem |
| C3604● data | Free-machining brass 58/3 (CZ121) | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu 57-59, Pb 2.5-3.5, Fe <= 0.3, Zn rem |
| C38000● data | Hot-stamping (forging) brass 58/2 | USA · UNS / ASTM B124, B283 | Wrought | Cu 55-60, Pb 1.5-2.5, Al <= 0.5, Zn rem |
| CW617N● data | CuZn40Pb2 | Europe · EN 1412 numbering | Wrought | Cu 57-59, Pb 1.6-2.5, Fe <= 0.3, Zn rem |
| 2.0402● data | CuZn40Pb2 | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu 57-59, Pb 1.6-2.5, Fe <= 0.3, Zn rem |
| CZ122● data | Hot-stamping (forging) brass 58/2 | UK · BS 2870-2875 | Wrought | Cu 57-59, Pb 1.6-2.5, Fe <= 0.3, Zn rem |
Overview
Free-cutting and forging brasses are copper-zinc alloys with about 1–3.7% lead added so that they machine with short, broken chips at high speed, and — in the forging grades — so that they can be hot stamped into near-net shapes. They are the most widely machined copper alloys in the world. Free-cutting brass C36000 (CW603N) and its European cousin CW614N (CuZn39Pb3) are the benchmark against which the machinability of every other copper alloy is measured, while CW617N (CuZn40Pb2) is the standard hot-stamping brass for valve bodies, gas fittings and cable glands.
The library covers the low-leaded, medium-leaded, free-cutting, riveting and forging brasses: C34000 / CW600N, C34200 / C35300 / CW601N, C36000 / CW603N, C35000 / CW606N, CW608N, C37700, CW612N, C38500 / CW614N and C38000 / CW617N, with their DIN, BS and JIS equivalents. This guide explains how they differ, how to choose between bar-turned and hot-stamped routes, and the regulatory points on lead that every buyer should check.
Why lead makes brass machine so well
Lead does not dissolve in brass. It stays as tiny, evenly spread globules between the grains. During cutting, these soft particles act as chip breakers and as a built-in lubricant at the tool tip. The chip snaps into small curls instead of forming long ribbons, cutting forces drop, heat falls, tools last longer and surface finish improves. A free-cutting brass can be turned several times faster than a plain brass, which is why screw-machine and CNC-turned brass parts are so economical.
The metallurgy in plain words
- Copper (about 55–65%) — sets the base. Higher copper means more ductility for cold heading and riveting; lower copper (about 57–60%) means more beta phase for hot working.
- Zinc (balance, about 35–42%) — gives strength and allows hot working. Grades with about 39–42% zinc are alpha-beta brasses that are very plastic when hot — the basis of hot stamping.
- Lead (about 0.8–3.7%) — controls machinability. About 1% gives modest improvement with good cold formability; 2% is a balance; 3% gives maximum machinability.
- Iron, tin, nickel, aluminum — limited as impurities, though small amounts of aluminum are permitted in some forging brasses to give a bright surface after stamping.
The grades compared
| USA | EN | Nominal type | Lead | Best route | Typical parts |
|---|---|---|---|---|---|
| C34000 | CW600N CuZn35Pb1 | Low-leaded brass | About 1% | Turning + cold forming, engraving | Cold-headed and knurled parts, engraved plates |
| C34200 / C35300 | CW601N CuZn35Pb2 | Medium-leaded brass | About 2% | Turning, knurling | Clock and instrument plates, knurled parts |
| C35000 | CW606N CuZn37Pb2 | Riveting / cold-heading brass | About 1–2% | Cold heading, riveting | Rivets, screws, cold-headed parts |
| C36000 | CW603N CuZn36Pb3 | Free-cutting brass (alloy 360) | About 2.5–3.7% | High-speed turning | Screw-machine parts, inserts, terminals, fasteners |
| C38500 | CW614N CuZn39Pb3 | Free-machining brass 58/3 | About 2.5–3.5% | Turning, light hot work | Turned parts, cable-gland bodies, inserts |
| — | CW608N CuZn38Pb2 | Leaded brass 38/2 | About 1.6–2.5% | Hot stamping + machining | Stampings, machined parts |
| C37700 | CW612N CuZn39Pb2 (near) | Forging brass 39/2 | About 1.5–2.5% | Hot stamping | Valve bodies, fittings, cable glands |
| C38000 | CW617N CuZn40Pb2 | Hot-stamping (forging) brass 58/2 | About 1.5–2.5% | Hot stamping | Valve bodies, gas and water fittings, cable glands |
Typical properties
Typical values from Copper Development Association and EN 12164 / EN 12165 data, given for orientation. The temper and size on your order and the governing standard set the actual values.
| Property | C36000 / CW614N bar (half-hard) | CW617N forgings | C34000 / CW600N |
|---|---|---|---|
| Tensile strength | Typically about 380–480 MPa | Typically about 350–450 MPa | Typically about 340–420 MPa |
| Elongation | About 10–25% | About 15–25% | Higher — suited to cold forming |
| Machinability rating (C36000 = 100) | 100 / about 90–100 | About 80–90 | About 60–70 |
| Electrical conductivity | About 25–28% IACS | ||
| Density | About 8.4–8.5 g/cm³ | ||
Bar turning versus hot stamping
Buyers often have a choice between machining a part fully from bar and hot stamping (forging) a near-net blank that is then machined. The right answer depends on shape and quantity:
| Machined from bar (C36000 / CW614N) | Hot stamped then machined (CW617N) | Cast then machined (leaded cast brass) | |
|---|---|---|---|
| Best shapes | Round, axisymmetric parts | Bodies with branches, hexes, flanges | Complex hollow bodies, larger parts |
| Tooling cost | None (only programs/fixtures) | Forging dies | Pattern or die |
| Material yield | Low for complex parts (lots of swarf) | High | High |
| Strength / soundness | Very good | Very good, dense grain flow | Good; porosity must be controlled |
| Typical quantity | Prototype to very high | Medium to very high | One-off to high |
For hollow or larger bodies — pump and valve housings, large fittings — casting in a leaded brass or gunmetal is often the better option. Conex offers sand, gravity die, low-pressure and pressure die casting for brass, followed by in-house CNC machining.
Lead and regulations — what buyers must check
- Drinking water. Many markets restrict lead in parts that touch potable water. In the USA, the Safe Drinking Water Act limits the weighted-average lead content of wetted surfaces to 0.25%, with certification usually to NSF/ANSI 61 and 372. In the EU, materials for drinking-water contact are moving to positive lists such as the 4MS common approach. Standard free-cutting brasses do not meet these limits — use lead-free or DZR grades approved for the market.
- Electrical and electronic equipment. The EU RoHS directive currently allows lead in copper alloys under a time-limited exemption that is reviewed periodically. Check the current status for your product category.
- Toys, food contact and consumer products may have their own lead limits.
Applications by industry
| Industry | Parts | Usual grades |
|---|---|---|
| Electrical & cable accessories | Cable-gland bodies, terminals, earthing fittings, inserts | CW614N, C36000, CW617N |
| Gas & water (non-potable) | Valve bodies, fittings, unions, adapters | CW617N, C37700 |
| Instrumentation | Fittings, manifolds, gauge parts | C36000, CW614N |
| Fasteners & hardware | Screws, nuts, rivets, threaded inserts | C36000, C35000, CW606N |
| Automotive | Sensor housings, connectors, fittings | CW614N, CW617N |
| Plastics & molding | Threaded inserts for molding | C36000, CW614N |
How to choose between grades
- Mostly turned and drilled? C36000 (USA) or CW614N (Europe, India).
- Turned and then crimped, knurled or cold headed? A lower-lead grade such as CW600N/C34000 or CW606N/C35000.
- Complex body with branches or hexes in volume? Hot stamping in CW617N.
- Drinking water or a lead-restricted market? Move to the DZR and lead-free brass category.
- Seawater or aggressive water? Leaded brasses are not suitable; consider naval brass, aluminum bronze or gunmetal.
Equivalents across standards
| USA | EN | DIN | BS | JIS |
|---|---|---|---|---|
| C38500 | CW614N CuZn39Pb3 | 2.0401 | CZ121 | C3603 / C3604 |
| C36000 | CW603N CuZn36Pb3 | 2.0375 | CZ124 | C3601 / C3602 |
| C38000 (near) | CW617N CuZn40Pb2 | 2.0402 | CZ122 | — |
| C34000 | CW600N CuZn35Pb1 | 2.0331 (near) | CZ118 | C3501 |
| C35000 | CW606N CuZn37Pb2 | — | CZ131 | C3713 |
"Near" means the compositions overlap but limits are not identical. Indian buyers often specify IS 319 free-cutting brass, which corresponds closely to the CW614N family.
Design and machining tips
- Design for bar size. Choose a hexagon or round that the part fits inside with minimum stock removal.
- Threads: free-cutting brass threads cleanly by cutting or rolling; avoid very fine threads in thin walls.
- Hot-stamped parts need draft (typically a few degrees) and generous radii, like castings.
- Plating: nickel and chrome plating are common; ask for lead-surface treatment if lead leaching is a concern.
- Stress-corrosion cracking: heavily machined or crimped parts used near ammonia should be stress relieved.
Common mistakes
- Using leaded brass for potable water where regulations require lead-free alloys.
- Crimping or bending C36000. High lead reduces cold ductility; cracks appear. Use a low-lead grade.
- Using forging brass in seawater or chloride service — dezincification and stress-corrosion cracking.
- Mixing US and EN designations on one drawing without stating which governs.
- Specifying bar-turned parts for complex hollow bodies when a casting or stamping would cut material waste dramatically.
Free-cutting versus forging brass
Free-cutting brass (C36000, CuZn39Pb3 / CW614N) is designed to be machined at high speed on automatic lathes. Its lead content breaks chips into small pieces, so it is the reference material for machinability, rated 100 on the common scale. Forging brass (C37700, CuZn40Pb2 / CW617N) has a structure that flows well when hot forged, so it is used for valve bodies, fittings and parts with shapes that would waste too much material if machined from bar. After forging, the parts are machined, and forging brass machines almost as well as free-cutting brass.
Choosing between bar and forging
For small, simple, round parts in high volumes, machining from free-cutting bar is fastest and needs no tooling. For larger or more complex shapes, especially with side outlets or flanges, hot forging saves material and gives dense, sound bodies that hold pressure well. Forging needs dies, so it suits medium and high volumes. Casting remains the route for very large or very complex shapes.
Lead limits and alternatives
For drinking water and some consumer products, lead content in brass may be restricted. Low-lead and lead-free brasses (silicon brasses such as CuZn21Si3P / CW724R, bismuth brasses and C69300) replace C36000 and CW617N in those applications, at some cost in machining speed.
Working with Conex on brass parts
Conex machines free-cutting brass parts from bar and machines forged and cast brass parts on in-house CNC lines in Jamnagar, supplying them with chemical analysis, dimensional reports and material certificates under an ISO 9001:2015 quality system to customers in more than 34 countries.
Typical brass parts
Fittings, adaptors, unions, valve stems and bodies, plumbing and gas parts, electrical terminals and connectors, fasteners and inserts, instrument parts, lock components, nozzles and decorative hardware are made in free-cutting and forging brass in very large numbers worldwide.
Ordering brass parts
Send the drawing with alloy, thread standards, finish or plating, any lead limit and annual quantity. For forged parts, the forging die can be planned once volumes are confirmed, and machined-from-bar samples supplied in the meantime.
Before you send an enquiry
A short list of facts helps choose the right grade from this family and quote accurately the first time:
- The part and its job: what it does, what it touches, and what a failure would cost in downtime or safety.
- Service conditions: fluid or environment, temperature range, pressure, loads, speed and lubrication.
- Grade or standard on the drawing: the UNS, EN, BS, JIS, GB, DIN or IS designation, or the old grade name if that is all you have.
- Process or stock form: sand, centrifugal, continuous, gravity die or investment casting, or bar and plate. The most economical route can be suggested for your quantity.
- Machining stage: rough cast, semi-finished with allowance, or fully finished to drawing.
- Tests and documents: chemical analysis, mechanical and hardness tests, pressure test, NDT, material test certificate type (EN 10204 3.1), dimensional report and any third-party inspection.
- Quantities and timing: prototype, first batch, annual volume and delivery schedule.
- Market rules: any lead limit, drinking-water approval, RoHS or REACH requirement in the destination market.
With these details, the grade can be confirmed against the options covered on this page, or an equivalent suggested where it gives better value or performance for the same job.
Frequently asked questions
What is the most machinable brass?
C36000 free-cutting brass (CW603N) and the closely related CW614N (CuZn39Pb3, BS CZ121). C36000 is the 100 reference point for copper-alloy machinability ratings.
What is the difference between CW614N and CW617N?
CW614N has about 3% lead and is optimized for machining from bar. CW617N has about 2% lead and slightly different copper and zinc so it hot stamps well; it is the standard forging brass for valve bodies and fittings.
Is free-cutting brass lead-free?
No. Free-cutting brasses contain about 1–3.7% lead. For lead-restricted uses, choose a lead-free bismuth or silicon brass.
Can free-cutting brass be used for drinking water?
Generally not in regulated markets such as the USA and the EU. Use an approved DZR or lead-free brass and the required certification.
Can I cast free-cutting brass?
Foundries use cast leaded brasses (such as C85700, C85800, CC754S) with similar machinability rather than wrought free-cutting compositions.
What is the Indian standard for free-cutting brass?
IS 319 covers free-cutting leaded brass bars, rods and sections; its main grade corresponds closely to CW614N / CZ121.
Why do brass forgings crack in service?
Usually stress-corrosion cracking caused by residual stress plus ammonia or other aggressive media, or dezincification in aggressive water. Stress relief and correct alloy selection prevent both.
What information do you need to quote a turned brass part?
The drawing, grade and standard, quantity per order and per year, finish or plating, thread and tolerance requirements, packing and the documents you need, such as an EN 10204 3.1 certificate.
Other brass categories
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.