34 grades · 8 cast · 26 wrought
Pure Copper
Unalloyed high-conductivity copper (ETP, OF, DHP) for electrical and thermal parts. 34 grades across USA, European, German, British, Japanese and Chinese standards — each with its own datasheet and cross-reference.
34 of 34 grades
| Grade | Name | System | Form | Composition |
|---|---|---|---|---|
| C80100● data | Cast copper 99.95 | USA · UNS | Cast | Cu ≥ 99.95 |
| C81100● data | Cast copper (HC) | USA · UNS | Cast | Cu ≥ 99.70 |
| CC040A● data | Cu-C | Europe · EN 1982:2017 | Cast | Cu ≥ 99.9 (cast from Cu-CATH-2 / Cu-ETP-2 / Cu-FRHC) |
| 2.0060 (approx.)● data | G-Cu | Germany · DIN 17655 | Cast | Cu ≥ 99.9 (conductivity grades G-CuL45/L50) |
| CAC101● data | CuC1 | Japan · JIS H 5120 | Cast | Cu ≥ 99.5 |
| CAC102● data | CuC2 | Japan · JIS H 5120 | Cast | Cu ≥ 99.7 |
| CAC103● data | CuC3 | Japan · JIS H 5120 | Cast | Cu ≥ 99.9 |
| ZCu99● data | ZCu99 | China · GB/T 1176-2013 | Cast | Cu ≥ 99.0 |
| C10100● data | Oxygen-free electronic copper | USA · UNS / ASTM B152, B187, B124 | Wrought | Cu >= 99.99, O <= 0.0005 |
| CW009A● data | Cu-OFE | Europe · EN 1412 numbering | Wrought | Cu >= 99.99, O <= 0.0005 |
| C110● data | Oxygen-free electronic copper | UK · BS 2870-2875 | Wrought | Cu >= 99.99, O <= 0.0005 |
| C1011● data | Oxygen-free electronic copper | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu >= 99.99, O <= 0.0005 |
| C10200● data | Oxygen-free copper | USA · UNS / ASTM B152, B187, B133 | Wrought | Cu >= 99.95, O-free |
| CW008A● data | Cu-OF | Europe · EN 1412 numbering | Wrought | Cu >= 99.95, O-free |
| 2.0040● data | OF-Cu | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu >= 99.95, O-free |
| C103● data | Oxygen-free copper | UK · BS 2870-2875 | Wrought | Cu >= 99.95, O-free |
| C1020● data | Oxygen-free copper | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu >= 99.95, O-free |
| C10300● data | Phosphorus-deoxidised high-conductivity copper | USA · UNS / ASTM B152 | Wrought | Cu >= 99.95, P 0.001-0.006 |
| CW020A● data | Cu-PHC | Europe · EN 1412 numbering | Wrought | Cu >= 99.95, P 0.001-0.006 |
| 2.0070● data | SE-Cu | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu >= 99.95, P 0.001-0.006 |
| C11000● data | Electrolytic tough-pitch copper (ETP) | USA · UNS / ASTM B152, B187, B124, B49 | Wrought | Cu >= 99.90, O 0.02-0.04 |
| CW004A● data | Cu-ETP | Europe · EN 1412 numbering | Wrought | Cu >= 99.90, O 0.02-0.04 |
| 2.0065● data | E-Cu58 | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu >= 99.90, O 0.02-0.04 |
| C101● data | Electrolytic tough-pitch copper (ETP) | UK · BS 2870-2875 | Wrought | Cu >= 99.90, O 0.02-0.04 |
| C1100● data | Electrolytic tough-pitch copper (ETP) | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu >= 99.90, O 0.02-0.04 |
| C12000● data | Deoxidised low-residual-P copper (DLP) | USA · UNS / ASTM B75, B152 | Wrought | Cu >= 99.90, P 0.005-0.013 |
| CW023A● data | Cu-DLP | Europe · EN 1412 numbering | Wrought | Cu >= 99.90, P 0.005-0.013 |
| 2.0076● data | SW-Cu | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu >= 99.90, P 0.005-0.013 |
| C1201● data | Deoxidised low-residual-P copper (DLP) | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu >= 99.90, P 0.005-0.013 |
| C12200● data | Deoxidised high-residual-P copper (DHP) | USA · UNS / ASTM B75, B88, B280, B152 | Wrought | Cu >= 99.90, P 0.015-0.040 |
| CW024A● data | Cu-DHP | Europe · EN 1412 numbering | Wrought | Cu >= 99.90, P 0.015-0.040 |
| 2.0090● data | SF-Cu | Germany · DIN 17660 / 17662 / 17663 / 17664 / 1766 | Wrought | Cu >= 99.90, P 0.015-0.040 |
| C106● data | Deoxidised high-residual-P copper (DHP) | UK · BS 2870-2875 | Wrought | Cu >= 99.90, P 0.015-0.040 |
| C1220● data | Deoxidised high-residual-P copper (DHP) | Japan · JIS H 3100 / H 3250 / H 3300 | Wrought | Cu >= 99.90, P 0.015-0.040 |
Overview
Pure copper is copper with at least 99.0–99.99% Cu and no deliberate alloying additions, chosen above all for its electrical and thermal conductivity. In the alloy library it covers two groups: cast high-conductivity copper (C80100, C81100, CC040A, CAC101–CAC103, ZCu99) and the wrought coppers that buyers know as ETP, OF, OFE, DLP and DHP (C11000, C10200, C10100, C12000, C12200 and their EN, DIN, BS and JIS equivalents). The grades differ mainly in how oxygen is removed or controlled, and that one difference decides how well the metal conducts, brazes, welds and casts.
This guide explains what separates one pure-copper grade from another, which grades suit cast parts and which suit machined bar and plate, how to read the equivalents across standards, and the design and ordering points that matter when you buy copper components from a foundry.
What counts as "pure" copper?
Every commercial copper contains small amounts of other elements. A grade is classed as unalloyed or "pure" copper when copper (sometimes counted together with silver) is at least 99.0–99.9%, and any other elements are either residual impurities or deliberate trace additions — usually oxygen or phosphorus — whose job is to control how the metal behaves during melting, not to strengthen it.
Two families sit in this category:
- Cast copper — poured into sand, centrifugal or continuous molds to make shaped parts such as electrical connectors, tuyeres, furnace cooling blocks and bus fittings. US designations are C80100 to C81100; Europe uses CC040A; Japan CAC101/102/103; China ZCu99; the UK HCC1.
- Wrought copper — rolled, drawn or extruded into bar, rod, strip, plate and tube, then machined. These are the C10100–C12200 series in the USA and the CW0xxA series in EN standards.
The metallurgy in plain words
Copper's conductivity is extremely sensitive to anything dissolved in it. Even a few hundredths of a percent of phosphorus, iron or silicon can lower conductivity by several percent IACS. That is why pure-copper grades are defined by how oxygen is handled:
Tough-pitch copper (ETP)
Electrolytic tough-pitch copper (C11000, CW004A, Cu-ETP) deliberately retains a small amount of oxygen, typically 0.02–0.04%. The oxygen ties up impurities as oxides, which keeps conductivity at or above 100% IACS. The drawback is hydrogen embrittlement: if ETP copper is heated in a hydrogen-bearing atmosphere (for example during brazing or welding with a reducing flame), hydrogen reacts with the oxide to form steam inside the metal and the part can crack.
Oxygen-free copper (OF and OFE)
Oxygen-free grades (C10200 / CW008A, and the electronic grade C10100 / CW009A) are melted and cast under protective conditions so that oxygen is essentially absent without adding a deoxidizer. They combine full conductivity with immunity to hydrogen embrittlement, which is why they are used for vacuum electronics, high-reliability conductors and parts that will be brazed in a hydrogen furnace. OFE adds tight limits on impurities and is the premium grade.
Phosphorus-deoxidized copper (DLP, DHP, PHC)
Here phosphorus is added to remove oxygen. A low residual phosphorus level (C12000 DLP, or the high-conductivity PHC grade C10300 / CW020A) keeps conductivity high. A higher residual phosphorus level (C12200 DHP, CW024A) makes the copper easy to weld and braze — it is the standard grade for plumbing and refrigeration tube — but conductivity falls to roughly 80–90% IACS.
Cast copper
Pure copper is one of the more difficult metals to cast. It has a high melting point (about 1,083 °C), it absorbs hydrogen and oxygen readily when molten, and its short freezing range makes it prone to shrinkage and gas porosity. The foundry has to deoxidize the melt carefully — usually with small amounts of boron, calcium boride, lithium or phosphorus — while keeping residuals low enough to protect conductivity. Grades such as C81100 and CC040A therefore specify minimum copper content and, in many specifications, a minimum conductivity rather than mechanical properties.
Grades in this category and how they differ
| Grade (USA) | Common name | Form | Key composition point | Main reason to choose it |
|---|---|---|---|---|
| C80100 | Cast copper 99.95 | Cast | Cu ≥ 99.95 | Highest-purity cast conductors |
| C81100 | Cast copper (HC) | Cast | Cu ≥ 99.70 | Practical high-conductivity castings: connectors, cooling blocks, tuyeres |
| C10100 | OFE (oxygen-free electronic) | Wrought | Cu ≥ 99.99, O ≤ 0.0005 | Vacuum and electronic parts, hydrogen brazing |
| C10200 | OF (oxygen-free) | Wrought | Cu ≥ 99.95, oxygen-free | Conductors that will be brazed or welded |
| C10300 | PHC | Wrought | P 0.001–0.006 | High conductivity plus weldability |
| C11000 | ETP | Wrought | O 0.02–0.04 | Busbars and general electrical parts — the default |
| C12000 | DLP | Wrought | P 0.005–0.013 | Good conductivity, better joining than ETP |
| C12200 | DHP | Wrought | P 0.015–0.040 | Tube, heat exchangers, brazed assemblies |
Typical properties
The values below are typical ranges drawn from published ASTM and Copper Development Association data for the grades named. They are for orientation only; the values that apply to your order are those in the specification called up on your drawing and in the material test certificate.
| Property | Cast copper (C81100 type) | Wrought ETP / OF, annealed | Wrought ETP / OF, hard drawn |
|---|---|---|---|
| Electrical conductivity | Typically about 85–92% IACS, depending on deoxidation and soundness | About 100–101% IACS | About 97–100% IACS |
| Tensile strength | Typically about 150–200 MPa | About 220–250 MPa | About 300–380 MPa |
| Elongation | High (ductile) | High (40%+) | Low to moderate |
| Thermal conductivity | High (somewhat below wrought) | About 390 W/m·K | About 390 W/m·K |
| Density | About 8.9 g/cm³ | ||
DHP copper (C12200) has similar strength to ETP but conductivity of roughly 80–90% IACS because of its residual phosphorus.
If conductivity matters, put a minimum % IACS on the drawing and ask for it to be measured and reported. A copper casting can meet its chemical analysis and still fall short on conductivity if it contains porosity or excess deoxidizer.
Casting methods that suit pure copper
- Sand casting — the usual route for connectors, terminals, cooling blocks and one-off or low-volume parts. Careful gating and risering are needed because of copper's shrinkage and gas pickup.
- Centrifugal casting — produces dense rings, sleeves and tubular blanks; centrifugal force pushes inclusions and gas toward the bore, where they are machined away.
- Continuous casting — used for solid and hollow bars that are then machined into parts.
- Investment casting — possible for small, intricate copper parts, though conductivity-critical parts are more often machined from wrought bar.
Many buyers combine both routes: shaped, heavy or hollow components are cast, while small, conductivity-critical parts are CNC machined from wrought C11000 or C10200 bar. Conex casts copper parts at its foundry in Jamnagar and machines both cast and wrought copper in-house.
Applications by industry
| Industry | Typical copper parts | Usual grades |
|---|---|---|
| Power transmission & distribution | Terminal lugs, bus connectors, clamps, earthing fittings | C81100, C11000 |
| Transformers & switchgear | Bushing stud connectors, terminal pads, flexible-link ends, busbar fittings | C11000, C10200, C81100 |
| Steel & metallurgy | Tuyeres, lances, furnace cooling staves and blocks | C81100, CC040A |
| Welding & resistance equipment | Electrode holders, current-carrying parts (strength-critical parts often move to chromium copper) | C11000, C10200 |
| Electronics & vacuum | Waveguides, vacuum-tube parts, high-reliability conductors | C10100, C10200 |
| HVAC & refrigeration | Tube, fittings, heat-exchanger parts | C12200 |
How to choose between grades
- Is the part shaped, hollow or large? If yes, a casting in C81100 / CC040A is usually the economical choice. If it is small and simple, machining from wrought bar may be cheaper and will give higher conductivity.
- Will it be brazed, welded or heated in a reducing atmosphere? Avoid ETP. Choose an oxygen-free grade (C10200) for conductors, or DHP (C12200) where conductivity is less critical.
- How much conductivity do you need? For 100% IACS, specify wrought ETP or OF. For cast parts, agree a realistic minimum with the foundry.
- Is strength important? Pure copper is soft. If the part must carry mechanical load or resist wear at temperature, look at the high-copper alloys (chromium copper C18200 / C81500, chromium-zirconium copper C18150) instead.
- Is it for vacuum or electronics? Specify OFE (C10100 / CW009A).
Equivalents across standards
The pairs below are widely accepted near-equivalents. Composition limits differ slightly between standards, so always quote the one standard that governs your order.
| USA (UNS) | EN | DIN (Werkstoff) | BS | JIS |
|---|---|---|---|---|
| C11000 (ETP) | CW004A Cu-ETP | 2.0065 E-Cu58 | C101 | C1100 |
| C10200 (OF) | CW008A Cu-OF | 2.0040 OF-Cu | C103 | C1020 |
| C10100 (OFE) | CW009A Cu-OFE | — | C110 | C1011 |
| C12000 (DLP) | CW023A Cu-DLP | 2.0076 SW-Cu | — | C1201 |
| C12200 (DHP) | CW024A Cu-DHP | 2.0090 SF-Cu | C106 | C1220 |
| C81100 / C80100 (cast) | CC040A Cu-C | G-Cu (approx.) | HCC1 | CAC101–CAC103 |
China's ZCu99 is the usual GB counterpart for cast copper.
Design and machining tips
- Keep sections uniform. Copper's short freezing range punishes abrupt changes in thickness. Blend sections with generous fillets and let the foundry place risers on the heavy areas.
- Allow machining stock on contact faces. Electrical contact faces are usually machined to remove the as-cast skin and expose dense metal; 2–3 mm per face is a common starting point for sand castings.
- Expect gummy machining. Pure copper is soft and ductile and tends to form long, stringy chips and built-up edge. Sharp, positive-rake tools, polished flutes, high cutting speeds and good coolant give the best results. Free-cutting tellurium copper (C14500) is the answer when machinability matters more than the last few percent of conductivity.
- Specify plating if needed. Tin or silver plating on contact surfaces reduces oxidation and contact resistance; state the thickness on the drawing.
- Threads and fasteners. Copper threads gall and strip easily; consider larger thread engagement, inserts, or bronze/stainless fasteners with anti-seize.
Common mistakes
- Ordering ETP for a brazed assembly. Hydrogen embrittlement can crack parts in service. Use OF or DHP.
- Expecting 100% IACS from a casting. Cast copper conducts very well but rarely matches wrought ETP. Agree the figure in advance.
- Writing "copper" without a grade. Always give a grade and standard — for example "C11000 to ASTM B187" or "CC040A to EN 1982".
- Using pure copper where strength is needed. Parts that are clamped, spring-loaded or hot need a high-copper alloy, not pure copper.
- Confusing DHP with high-conductivity copper. C12200 is excellent for tube and brazing but not for busbars.
Quality checks and documents
For copper parts Conex typically provides chemical analysis by spectrometer, dimensional inspection against your drawing, visual inspection of surfaces and, where requested, conductivity measurement, hardness and other tests called up by the specification. Material test certificates are issued with each shipment, and inspection is carried out under an ISO 9001:2015 quality system.
Frequently asked questions
Which copper grade has the highest electrical conductivity?
Oxygen-free electronic copper (C10100 / CW009A) and ETP copper (C11000 / CW004A) both reach about 100–101% IACS. OFE has the tightest impurity control and is used where purity and vacuum performance matter.
Can pure copper be cast?
Yes. Grades such as C81100 and CC040A are cast in sand, centrifugal and continuous processes. It is harder to cast than brass or bronze because of gas pickup and shrinkage, so the foundry's melting and deoxidation practice is critical.
What conductivity can I expect from a copper casting?
Well-made high-conductivity copper castings typically reach the mid-80s to low-90s % IACS. Put your minimum on the drawing and ask for it to be measured.
What is the difference between C11000 and C12200?
C11000 (ETP) contains a little oxygen and has the highest conductivity but cannot be safely brazed in hydrogen. C12200 (DHP) is deoxidized with phosphorus, so it brazes and welds well, but its conductivity is lower. Use C11000 for busbars and C12200 for tube and brazed parts.
What is the European equivalent of C11000?
CW004A (Cu-ETP) to EN 1652, EN 12163 and related standards. The older DIN equivalent is 2.0065 (E-Cu58), and the BS equivalent is C101.
Is pure copper strong enough for clamps and connectors?
For light-duty conductors, yes. For parts that are bolted tightly, carry spring load or run hot, a high-copper alloy such as chromium copper or chromium-zirconium copper keeps its strength far better while still conducting well.
Why is my copper difficult to machine?
Pure copper is soft and ductile, so it smears and forms long chips. Use sharp, positive-rake tools and high speeds, or choose tellurium copper (C14500) for free machining if a small loss of conductivity is acceptable.
What should I put on my drawing when ordering copper castings?
The grade and standard, any minimum conductivity, critical dimensions and tolerances, machined faces, plating, the quantity and the inspection documents you need (for example a material test certificate to EN 10204 3.1).
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.