ConexCONEXCASTING FOUNDRY

14 grades · 14 cast

Aluminum Die-Casting Alloys

High-pressure die-casting alloys (A380 / ADC12 / LM24 / A413). 14 grades across USA, European, German, British, Japanese and Chinese standards — each with its own datasheet and cross-reference.

Al-Si11Cu2(Fe) die-casting (383 / ADC12) · 5Al-Si9Cu3(Fe) die-casting (A380 / ADC10) · 6Al-Si9Cu3(Fe)(Zn) die-casting (LM24) · 3

14 of 14 grades

GradeNameSystemFormComposition
383.0● data383.0USA · AA cast alloy designationCastSi 10-12, Cu 1.5-3.5, Fe <= 1.1, Zn <= 1.7, Al rem
A380.0● dataA380.0USA · AA cast alloy designationCastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 1.2, Al rem
EN AC-46000● dataEN AC-AlSi9Cu3(Fe)Europe · EN 1706:2020+A1:2021CastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 1.2, Al rem
EN AC-46100● dataEN AC-AlSi11Cu2(Fe)Europe · EN 1706:2020+A1:2021CastSi 10-12, Cu 1.5-3.5, Fe <= 1.1, Zn <= 1.7, Al rem
EN AC-46500● dataEN AC-AlSi9Cu3(Fe)(Zn)Europe · EN 1706:2020+A1:2021CastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 3.0, Al rem
G-AlSi9Cu3● dataG-AlSi9Cu3Germany · DIN legacy aluminum casting symbolsCastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 1.2, Al rem
GD-AlSi9Cu3● dataGD-AlSi9Cu3Germany · DIN legacy aluminum casting symbolsCastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 1.2, Al rem
LM2● dataLM2UK · BS 1490CastSi 10-12, Cu 1.5-3.5, Fe <= 1.1, Zn <= 1.7, Al rem
LM24● dataLM24UK · BS 1490CastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 3.0, Al rem
ADC10● dataADC10Japan · JIS H 5302CastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 1.2, Al rem
ADC10Z● dataADC10ZJapan · JIS H 5302CastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 3.0, Al rem
ADC12● dataADC12Japan · JIS H 5302CastSi 10-12, Cu 1.5-3.5, Fe <= 1.1, Zn <= 1.7, Al rem
YL112● dataYL112China · GB/T 15115CastSi 8-11, Cu 2-4, Fe <= 1.3, Zn <= 1.2, Al rem
YL113● dataYL113China · GB/T 15115CastSi 10-12, Cu 1.5-3.5, Fe <= 1.1, Zn <= 1.7, Al rem

Overview

Aluminum die-casting alloys are aluminum-silicon-copper alloys — typically about 8–12% silicon and 1.5–4% copper, with relatively high iron — formulated for high-pressure die casting, where molten metal is injected at high speed and pressure into steel dies to make thin-walled, accurate, high-volume parts. The most widely used grades worldwide are A380 (EN AC-46000, ADC10) and 383 (ADC12, EN AC-46100), with the British LM24 and LM2 and the European AlSi9Cu3(Fe)(Zn) EN AC-46500 as close relatives. They are the standard materials for automotive housings, gearbox and engine covers, electrical enclosures, motor housings, power-tool bodies, lighting and consumer-product castings.

This guide explains why die-casting alloys differ from gravity and sand-casting alloys, how the grades compare, their typical properties and limits, and the design and specification points that matter for die-cast parts.

Why die-casting alloys have different chemistry

High-pressure die casting fills a steel die in milliseconds and freezes the metal very quickly. The alloy must flow into thin sections, not solder (stick) to the steel die, resist hot cracking and give a sound skin. The chemistry is tuned for this:

  • Silicon (about 8–12%) — gives excellent fluidity and reduces shrinkage and hot cracking.
  • Copper (about 1.5–4%) — adds strength and hardness in the as-cast condition and improves machinability; it reduces corrosion resistance.
  • Iron (up to about 1.1–1.3%) — deliberately higher than in gravity alloys because it prevents the aluminum from soldering to the steel die.
  • Zinc, magnesium, manganese, nickel — present within limits, often from recycled metal; zinc is allowed higher in some grades (AlSi9Cu3(Fe)(Zn)).

Most die-casting alloys are made largely from recycled aluminum ("secondary" alloys), which makes them economical and lowers their carbon footprint.

The grades compared

Grade (AA)EN ACDIN / BS / JIS / GBSilicon / copperMain characterTypical uses
A380.046000 AlSi9Cu3(Fe)GD-AlSi9Cu3 / — / ADC10 / YL112Si 8–11 / Cu 2–4The general-purpose die-casting alloy — balance of castability, strength and machinabilityHousings, covers, brackets, motor and gearbox parts
383.046100 AlSi11Cu2(Fe)— / LM2 (near) / ADC12 / YL113Si 10–12 / Cu 1.5–3.5Higher silicon — better fluidity and hot-crack resistance for thin, intricate partsThin-wall housings, electronics enclosures, complex parts
—46500 AlSi9Cu3(Fe)(Zn)LM24 (near) / ADC10ZSi 8–11 / Cu 2–4, Zn up to 3Variant of 46000 allowing higher zincGeneral die castings

Equivalents are close but not identical, especially in iron, zinc and impurity limits. Quote the governing standard (for example EN 1706, ASTM B85, JIS H5302).

Typical properties

Typical as-cast values for high-pressure die castings from ASTM B85 and EN 1706 data; actual values depend strongly on wall thickness, porosity and die design. Die-casting properties are usually measured on separately cast test bars or agreed sample locations.

PropertyA380 / AlSi9Cu3(Fe)383 / ADC12
Tensile strengthTypically about 240–330 MPaTypically about 230–310 MPa
0.2% proof strengthTypically about 140–170 MPaTypically about 140–160 MPa
ElongationAbout 1–4%About 1–3.5%
HardnessAbout 75–90 HBAbout 75–85 HB
DensityAbout 2.7–2.8 g/cm³
Thermal conductivityAbout 100–110 W/m·K
Standard high-pressure die castings are not normally heat treated: gas trapped during injection expands and causes surface blisters at solution-treatment temperatures. If you need high ductility or heat-treated strength, consider gravity die or low-pressure casting in A356 / LM25, or vacuum die casting with special alloys.

Die casting versus gravity die and sand casting

AspectHigh-pressure die casting (A380 / ADC12)Gravity die casting (LM6 / LM25)Sand casting
Minimum wallAbout 1.5–3 mmAbout 3–4 mmAbout 4–5 mm
Dimensional accuracyBest (about ISO 8062 DCTG 4–6)Good (DCTG 7–9)Moderate (DCTG 9–11)
Surface finishVery smoothGoodRougher
Tooling costHighestMediumLowest
Economic quantityHigh volumesMedium volumesOne-off to medium
Heat treatableNormally noYes (LM25 / A356)Yes (LM25 / A356)
DuctilityLowMedium–goodMedium
Pressure tightnessGood with impregnationVery goodGood

Conex casts aluminum by pressure die, gravity die, low-pressure and sand processes, so the process and alloy can be matched to the part's volume and duty, with CNC machining done in-house.

Applications by industry

IndustryParts
Automotive & EVGearbox and clutch housings, engine covers, brackets, motor and inverter housings
ElectricalJunction boxes, enclosures, motor end shields, lighting housings and heat sinks
Power tools & appliancesTool bodies, gear cases, appliance frames
Pumps & compressorsSmall pump and compressor housings, covers
Telecom & electronicsRadio and electronics enclosures, heat sinks
Furniture & hardwareChair bases, handles, fittings

How to choose

  1. General die castings with balanced properties? A380 / AlSi9Cu3(Fe) / ADC10.
  2. Very thin, intricate parts or crack-sensitive designs? 383 / ADC12.
  3. Corrosive or outdoor service? Copper-bearing alloys corrode faster — coat the parts or consider a low-copper alloy.
  4. Need ductility, weldability or heat treatment? Choose gravity or low-pressure casting in A356 / LM25.
  5. Low or medium volume? Gravity die or sand casting usually costs less overall because tooling is cheaper.

Design tips for die castings

  • Uniform, thin walls (typically 2–4 mm) cast best; thick sections trap porosity.
  • Draft of about 1–2° on outer walls and more on inner walls and cores.
  • Ribs instead of thickness for stiffness.
  • Generous radii at corners to help metal flow and die life.
  • Machining allowance small (about 0.5–1 mm) — machine as little as possible because the dense skin is the strongest layer and machining can expose porosity.
  • Leak-tight parts: specify vacuum impregnation where needed.
  • Ejector-pin and parting-line locations should be agreed so they do not land on cosmetic or sealing faces.

Common mistakes

  • Ordering T6 heat treatment for standard die castings — they will blister.
  • Designing thick sections in a die casting and expecting no porosity.
  • Using die-casting alloys for parts that need elongation or must be welded.
  • Machining away the cast skin on sealing faces and exposing porosity without impregnation.
  • Specifying wrought alloy names (6061) for die castings — they cannot be die cast.

Quality checks and documents

Each melt is analyzed by spectrometer; castings are inspected visually and dimensionally, X-rayed for porosity on critical areas, and leak tested where required. Impregnation, machining and coating are verified against the drawing. Material test certificates (EN 10204 3.1 on request) and inspection reports are supplied under an ISO 9001:2015 quality system.

Ordering checklist

  • 3D model and drawing with critical dimensions, cosmetic faces and sealing faces.
  • Alloy and standard (for example EN AC-46000 to EN 1706, or A380 to ASTM B85).
  • Annual volume and batch size — this decides die design and number of cavities.
  • Leak test, impregnation and X-ray requirements.
  • Machining, surface treatment (powder coat, paint, chromate-free conversion) and assembly.
  • Documents required, including first-article or PPAP for automotive customers.

Porosity in die castings and how to manage it

High-pressure die casting fills the die in milliseconds, which traps some air and die-lubricant gas inside the casting. This gas porosity is normal and usually sits in the thicker sections. It rarely matters for housings and covers, but it matters a great deal if the part must hold pressure, be heat treated, be welded or be machined deeply into thick walls. Several measures keep porosity under control: uniform wall thickness, generous radii, well-placed overflows and vents, vacuum-assisted die casting for critical parts, and keeping machining allowances small so the dense surface skin is not removed. Where pressure tightness is required, castings can be vacuum impregnated with a sealant after machining.

Ordinary high-pressure die castings are generally not heat treated to T6, because trapped gas expands at solution-treatment temperature and blisters the surface. If you need T6 strength, consider gravity die or low-pressure casting in A356 / LM25, or a vacuum die-casting process designed for heat treatment.

Surface finishing

Die castings have a smooth as-cast surface that takes paint and powder coating well. Common finishes include shot blasting, vibratory finishing, chromate-free conversion coating, powder coating and wet paint. Decorative anodizing is difficult on high-silicon die-casting alloys such as ADC12 / A383, because silicon darkens the anodic film and gives a gray, uneven appearance; low-silicon alloys or different processes are better when an anodized look is needed.

Tooling, volumes and cost

A die-casting die is a precision steel tool and represents a significant up-front cost. Die casting becomes economical at medium and high volumes, typically thousands of parts per year and upward, because the cycle time per part is short and machining can be minimal. For lower volumes, gravity die casting or sand casting in similar alloys is often more economical, and the part can move to die casting later if volumes grow. Buyers should share realistic annual quantities so the right process can be recommended.

Specifying die-casting alloys on a drawing

Callouts should name the alloy and standard, for example "Aluminum die-casting alloy ADC12 to JIS H5302" or "A380 to ASTM B85" or "EN AC-46000 to EN 1706". Add the general tolerance standard (for example ISO 8062 for castings), surface finish requirements, porosity acceptance criteria for machined faces, any leak test pressure, and the finish or coating.

Working with Conex on die castings

Conex produces aluminum castings by pressure die, gravity die, low-pressure and sand casting in Jamnagar, so the process can be matched to the part and the volume. Castings can be machined in-house on CNC equipment, leak tested where needed and supplied with inspection reports and material certificates under an ISO 9001:2015 quality system to customers in more than 34 countries.

Die-casting alloy chemistry in practice

Die-casting alloys contain more iron than gravity casting alloys on purpose: iron reduces the tendency of molten aluminum to stick to the steel die (soldering), which protects the tool and keeps cycle times short. The trade-off is lower ductility, because iron forms brittle needle-shaped compounds. Silicon improves fluidity so thin walls fill completely, and copper adds strength and hardness. Alloys such as A380 and ADC12 balance these elements for general use, while A360 and similar grades with less copper offer better corrosion resistance. Buyers needing higher elongation for crash or impact parts should discuss special low-iron, high-ductility die-casting alloys with the foundry.

Machining die castings

Die castings are designed to need little machining, but bores, sealing faces and threads are usually finished on CNC machines. Because the dense skin is only a few tenths of a millimeter thick, machining allowances should be kept small, typically 0.3 to 0.8 mm, to avoid opening up porosity. Locating datums should be cast features that are stable and easy to clamp.

Leak testing and impregnation

Housings for pumps, compressors, gearboxes and electrical equipment often must be oil or gas tight. Die castings for such parts are commonly air-decay or helium leak tested after machining. Parts that show small leaks through micro-porosity can be vacuum impregnated with a sealing resin and retested, a well-established process accepted by many OEMs. The leak test method, pressure and acceptance limit should be stated on the drawing.

Sharing volumes early

Annual quantity, part weight and the number of variants decide whether a die is worth making, so share them with the first drawing.

Before you send an enquiry

A short list of facts helps choose the right grade from this family and quote accurately the first time:

  • The part and its job: what it does, what it touches, and what a failure would cost in downtime or safety.
  • Service conditions: fluid or environment, temperature range, pressure, loads, speed and lubrication.
  • Grade or standard on the drawing: the UNS, EN, BS, JIS, GB, DIN or IS designation, or the old grade name if that is all you have.
  • Process or stock form: sand, gravity die, low-pressure or pressure die casting, or bar, plate and extrusion. The most economical route can be suggested for your quantity.
  • Machining stage: rough cast, semi-finished with allowance, or fully finished to drawing.
  • Tests and documents: chemical analysis, mechanical and hardness tests, pressure test, NDT, material test certificate type (EN 10204 3.1), dimensional report and any third-party inspection.
  • Quantities and timing: prototype, first batch, annual volume and delivery schedule.
  • Market rules: any lead limit, drinking-water approval, RoHS or REACH requirement in the destination market.

With these details, the grade can be confirmed against the options covered on this page, or an equivalent suggested where it gives better value or performance for the same job.

Frequently asked questions

What is the most common aluminum die-casting alloy?

A380 (EN AC-46000 AlSi9Cu3(Fe), JIS ADC10) in North America and Europe, and ADC12 (383) in Japan, China and much of Asia.

What is the difference between ADC10 and ADC12?

ADC12 has more silicon (about 10–12% against 8–11%), giving better fluidity for thin, complex parts; ADC10 has slightly higher copper and strength. Both are widely used.

Can die-cast aluminum be heat treated?

Normally no. Entrapped gas causes blisters during solution treatment. Low-temperature stress relief or aging may be possible in some cases.

Is A380 corrosion resistant?

Moderately. Its copper content reduces corrosion resistance compared with copper-free alloys, so outdoor parts are usually coated.

Can die castings be welded?

Generally not reliably, because of porosity. Mechanical joining or adhesive bonding is preferred.

What is LM24?

A British die-casting alloy close to AlSi9Cu3(Fe)(Zn) (EN AC-46500) and to A380.

When is die casting not the right process?

When quantities are low, parts are very large or thick, or the part needs high ductility, weldability or heat treatment. Gravity die or sand casting is then usually better.

Send your drawing, get a quotation.

DWG, PDF, STEP or a sample photo — with quantity and destination port.

All productsGet quote
☎Call✉Email⬇CatalogueGet Quote
Conex

Conex Export Desk

Talk to our export team

Working on a new casting? Tell us the part and we'll connect you with the right engineer today.