5 grades · 5 wrought
Pure Aluminum (1xxx)
Commercially pure aluminum for busbar, sheet and spinning. 5 grades across USA, European, German, British, Japanese and Chinese standards — each with its own datasheet and cross-reference.
5 of 5 grades
| Grade | Name | System | Form | Composition |
|---|---|---|---|---|
| 1050A● data | A91050 | USA · Aluminum Association / ASTM B209, B211, | Wrought | Al >= 99.5 |
| EN AW-1050A● data | EN AW-Al99,5 | Europe · EN 573-3 / EN 485 / EN 755 | Wrought | Al >= 99.5 |
| 3.0255● data | Al99.5 | Germany · DIN 1712 / 1725-1 | Wrought | Al >= 99.5 |
| 1B● data | Commercially pure 1050A | UK · BS 1470-1475 | Wrought | Al >= 99.5 |
| A1050● data | Commercially pure 1050A | Japan · JIS H 4000 / H 4040 | Wrought | Al >= 99.5 |
Overview
Pure aluminum (the 1xxx series) is commercially pure aluminum with at least 99.0% aluminum — 99.5% in the most common grade, 1050A — chosen for its high electrical and thermal conductivity, excellent corrosion resistance, outstanding formability and weldability, and its bright appearance after anodizing. It is not a strength material: annealed 1050A is one of the softest engineering metals. It is used for busbars and electrical conductors, chemical and food-processing equipment, heat-exchanger fins, reflectors, signage, cladding and deep-drawn or spun parts.
The library lists the one key grade in this series under its five common designations: 1050A (Aluminum Association), EN AW-1050A (EN 573), 3.0255 (DIN), 1B (BS) and A1050 (JIS). This guide explains what the last digits mean, how tempers change the properties, how 1050A compares with other conductor and structural aluminum alloys, and what to consider when machining or fabricating it.
How the 1xxx numbering works
In the international four-digit system for wrought aluminum, the first digit 1 means "99.0% aluminum or more". The last two digits give the minimum aluminum content beyond 99%: 1050 means at least 99.50% Al, 1100 at least 99.00%, 1070 at least 99.70%. The second digit shows impurity control — 0 means natural impurity limits; other digits indicate special control of one or more impurities. The "A" in 1050A indicates a national variation registered in Europe, very close to US 1050. A related grade, 1350 (formerly "EC" — electrical conductor), is optimized for conductivity and is the standard material for aluminum wire and many busbars.
The metallurgy in plain words
- Aluminum (≥ 99.5%) — light (density about 2.70 g/cm³), highly conductive and protected by a thin, tough natural oxide film that resists corrosion in air, water and many chemicals.
- Iron and silicon — the main impurities. They form small particles that slightly raise strength and reduce conductivity.
- No deliberate alloying — so 1xxx alloys cannot be heat treated for strength. They are strengthened only by cold work (rolling, drawing), described by "H" tempers.
Tempers and typical properties
Typical values from EN 485 / EN 754 and Aluminum Association data for 1050A; the governing standard and certificate apply.
| Temper | Meaning | Tensile strength | 0.2% proof strength | Elongation |
|---|---|---|---|---|
| O | Annealed (softest) | About 65–95 MPa | About 20–30 MPa | About 25–40% |
| H12 / H22 | Quarter hard | About 85–125 MPa | About 55–75 MPa | About 5–12% |
| H14 / H24 | Half hard | About 105–145 MPa | About 75–100 MPa | About 3–8% |
| H18 | Full hard | About 135+ MPa | About 120+ MPa | Low |
| Physical property | Typical value for 1050A |
|---|---|
| Electrical conductivity | About 59–62% IACS (about 34–36 MS/m) |
| Thermal conductivity | About 220–230 W/m·K |
| Density | About 2.70 g/cm³ |
| Melting range | About 645–658 °C |
Pure aluminum compared with other options
| Need | 1050A / 1350 | 6101 / 6063 (Al-Mg-Si) | Copper C11000 |
|---|---|---|---|
| Conductivity | Highest of aluminum alloys (about 60–62% IACS) | Slightly lower (about 50–57% IACS) | About 100% IACS |
| Strength | Low | Moderate to good after heat treatment | Moderate |
| Weight | Very light | Very light | Heavy |
| Formability | Excellent | Good | Excellent |
| Machinability | Poor (gummy) | Good | Fair |
| Typical use | Busbars, foil, fins, chemical tanks | Structural busbars, extrusions, heat sinks | Compact, high-current conductors, connectors |
Where pure aluminum fits in a foundry and machining supply chain
The 1xxx series is a wrought family: it is supplied as sheet, plate, strip, foil, bar, wire and extrusions. Pure aluminum is rarely used for castings because it has poor fluidity and high shrinkage compared with silicon-containing casting alloys; where a cast aluminum conductor or housing is needed, foundries use high-conductivity casting compositions or Al-Si alloys such as A356 or LM6. Buyers typically meet 1050A as:
- Busbars, flexible links and terminal plates machined, drilled and punched from bar or plate.
- Chemical and food equipment parts — tanks, liners, trays — fabricated by forming and welding.
- Components in assemblies where Conex supplies cast or machined copper-alloy connectors to join aluminum conductors.
Joining aluminum conductors to copper requires care: bimetallic connectors, tin-plated contact surfaces or approved compounds prevent galvanic corrosion and creep loosening at bolted joints. Conex manufactures cast and machined copper-alloy and aluminum connector components for these applications.
Applications by industry
| Industry | Parts |
|---|---|
| Power & electrical | Busbars, flexible links, conductor strip, transformer windings (foil) |
| Chemical & food processing | Tanks, linings, trays, equipment parts in contact with foods and certain chemicals |
| HVAC & heat transfer | Heat-exchanger fins, foil, cooling plates |
| Lighting & signage | Reflectors, nameplates, anodized panels |
| Packaging | Foil, containers, closures |
| Architecture | Cladding, roofing, decorative anodized parts |
How to choose a 1xxx grade and temper
- Maximum conductivity for electrical use? 1350 or 1050A in O or H temper as required for bending.
- Deep drawing or spinning? 1050A in the O temper.
- Flat parts needing some stiffness? H14 or H24.
- Need strength or machinability? Move to the 6xxx series (6061, 6082) or, for conductors, 6101.
- Bright decorative anodizing? High-purity 1xxx grades give the brightest finish.
Equivalents across standards
| AA (USA) | EN 573 | DIN | BS (old) | JIS |
|---|---|---|---|---|
| 1050 / 1050A | EN AW-1050A (Al 99.5) | 3.0255 | 1B | A1050 |
Indian Standard IS 737 also covers wrought aluminum sheet and strip in this purity class, where the grade is commonly referred to as 19500.
Machining and fabrication tips
- Machining: pure aluminum is soft and gummy and forms built-up edge. Use very sharp, polished, high-positive-rake tools (often uncoated carbide or PCD), high speeds and good lubrication or mist coolant. Harder tempers (H14, H18) machine better than O.
- Bending and punching: excellent in O and H1x tempers; burrs can be large — deburr contact surfaces.
- Welding: readily welded by TIG and MIG using 1xxx or 4xxx filler; strength in the weld zone falls to the annealed level.
- Electrical joints: clean the oxide, use contact compound or plating, and use spring washers or appropriate torque to manage creep.
- Anodizing: gives a clear, bright protective layer; specify thickness and color.
Electrical design notes for aluminum conductors
When aluminum replaces copper in a busbar or link, three points need attention. First, the cross-section must increase — roughly 1.6 times the copper area for similar resistance — so check space and clearances. Second, bolted joints must be designed for aluminum's lower hardness and its tendency to creep under sustained pressure: use larger contact areas, spring or conical washers, and the torque recommended for aluminum. Third, the surface oxide must be removed and the joint protected with contact grease or plating (tin or silver) so that resistance stays low over time. At transitions to copper, use bimetallic plates or tin-plated copper to avoid galvanic corrosion.
Corrosion resistance in more detail
Pure aluminum is protected by a thin, continuous oxide film that reforms instantly if scratched. It performs very well in rural, urban and many industrial atmospheres, in fresh water and in contact with many foods and chemicals, including concentrated nitric acid and many organic compounds. It is attacked by strong alkalis (such as caustic soda) and by strong acids like hydrochloric acid, and it should be isolated from copper and copper-bearing water to prevent pitting.
Common mistakes
- Using 1050A where strength is needed — it bends and creeps under load. Use 6xxx.
- Bolting aluminum directly to copper without a bimetallic interface or plating.
- Expecting easy machining — 1xxx is among the hardest aluminum grades to machine cleanly.
- Specifying a grade without a temper.
- Trying to cast pure aluminum for complex parts — use a casting alloy.
Quality checks and documents
For machined aluminum parts Conex verifies the material against the mill certificate, checks dimensions and finish against the drawing, and supplies an inspection report and material test certificate (EN 10204 3.1 on request) under an ISO 9001:2015 quality system. Conductivity measurement can be arranged for electrical parts.
Ordering checklist for machined aluminum parts
- Drawing or 3D model with tolerances, surface finish and any flatness or straightness requirements.
- Alloy and temper — for example 1050A-H14 to EN 573/EN 485 — and the governing standard (EN 573/EN 755, ASTM B211/B221/B209, IS 733/737).
- Form of supply if it matters: drawn bar, extruded bar, rolled plate or sheet.
- Surface treatment: anodizing type and thickness, conversion coating, paint or plating, and masking requirements.
- Quantity per batch and per year.
- Documents: mill certificate traceability, EN 10204 3.1 certificate, dimensional report.
What 1xxx alloys are good at
1xxx aluminum is at least 99 percent pure. It has the highest electrical and thermal conductivity of any aluminum series, excellent corrosion resistance and outstanding formability, but low strength. 1050 and 1060 are used for chemical tanks, heat exchanger fins, reflectors and deep-drawn parts; 1350 (EC grade) is the standard electrical conductor alloy for busbars, cables and windings; 1100 is a general-purpose grade with slightly more strength.
Electrical uses
Busbars, cable conductors, transformer windings, motor rotor cages and earthing strips use high-purity aluminum where weight and cost matter more than the higher conductivity of copper. Aluminum conducts about 61 percent as well as copper by volume but is much lighter, so an aluminum conductor of equal resistance weighs roughly half as much. Joints need care because aluminum forms a hard oxide and creeps under bolt pressure; correct connectors, contact compound and bolting practice are essential.
Specifying 1xxx
Examples: "1050A-H14 sheet to EN 485", "1350-H19 busbar to ASTM B236", "1100-O to ASTM B209". State conductivity if critical, for example a minimum of 61 percent IACS for 1350 busbar.
Working with Conex on aluminum parts
Conex machines aluminum busbar, plate and bar parts and casts aluminum alloys in Jamnagar, with certificates and inspection reports under an ISO 9001:2015 quality system for customers in more than 34 countries.
Before you send an enquiry
A short list of facts helps choose the right grade from this family and quote accurately the first time:
- The part and its job: what it does, what it touches, and what a failure would cost in downtime or safety.
- Service conditions: fluid or environment, temperature range, pressure, loads, speed and lubrication.
- Grade or standard on the drawing: the UNS, EN, BS, JIS, GB, DIN or IS designation, or the old grade name if that is all you have.
- Process or stock form: sand, gravity die, low-pressure or pressure die casting, or bar, plate and extrusion. The most economical route can be suggested for your quantity.
- Machining stage: rough cast, semi-finished with allowance, or fully finished to drawing.
- Tests and documents: chemical analysis, mechanical and hardness tests, pressure test, NDT, material test certificate type (EN 10204 3.1), dimensional report and any third-party inspection.
- Quantities and timing: prototype, first batch, annual volume and delivery schedule.
- Market rules: any lead limit, drinking-water approval, RoHS or REACH requirement in the destination market.
With these details, the grade can be confirmed against the options covered on this page, or an equivalent suggested where it gives better value or performance for the same job.
Frequently asked questions
What is 1050A aluminum?
A commercially pure aluminum with at least 99.5% Al, used for electrical conductors, chemical and food equipment, heat-exchanger fins and decorative parts.
Is 1050A good for busbars?
Yes, especially where maximum conductivity and easy bending matter. Where more strength is needed, 6101 is often used.
Can 1050A be heat treated?
No. It has no strengthening alloy additions and is hardened only by cold work (H tempers). Heating anneals it to the soft O temper.
What is the difference between 1050 and 1100?
1050 has at least 99.5% aluminum; 1100 has at least 99.0% and a little copper, giving slightly higher strength and slightly lower conductivity.
Is pure aluminum corrosion resistant?
Very — it has the best general corrosion resistance of the aluminum alloys in most atmospheres and many chemicals.
How does aluminum compare with copper as a conductor?
By cross-section it conducts about 60% as well; by weight it conducts about twice as well. Copper is chosen where space is limited, aluminum where weight and cost matter.
Why is pure aluminum hard to machine?
It is soft and ductile, so it sticks to cutting tools. Sharp, polished tools, high speeds and lubrication help; harder tempers machine better.
Other aluminum categories
Send your drawing, get a quotation.
DWG, PDF, STEP or a sample photo — with quantity and destination port.